2 Shot Molding

By TVP
Published: January 27th, 2012

I'm looking for a good book or resource on 2-shot molding.  Speficially on interaction/bonding/sealing between the shots and tests to prove the strength of the bond in different environmental scenarios.
 
Thanks in advance for the help!

Now that was a really healthy

Now that was a really healthy dialogue right there. Gets your blood pumping really fast and strong. Thanks a lot for sharing this with us. allergies talking

usually if you can't blend

usually if you can't blend them in a molding machine you won't get a chemical bond in two shot. SOLUTION? look for mechanical bonding (undercuts, through holes etc.)

Bill, Are you saying mix the

Bill,

Are you saying mix the pellets together and mold them, and if they delaminate then they won't bond?

Thanks!

RULE OF THUMB: If you can mix

RULE OF THUMB:
If you can mix it together and it doesn't separate you can use it for two color. IF you can't 'alloy' it, you need to design some mechanical undercuts.

Worse case is an adhesive overcoat on the first shot.

Hi I'm using a great source

Hi I'm using a great source in Taiwan. Great selection of Taiwanese 2 shot machines for trials.
Contact Avon Wang.
http://www.taiwan-chernliang.com/
chern.liang@msa.hinet.net
avonwang0714@gmail.com

Andy

Resin companies are a good

Resin companies are a good source.

Keep on 2 shot molding!

brent

Media Kit  |  Privacy Policy  |  Contact  |  Feedback  |  Subscribe | | |

© 2011 UBM Canon | please visit these other sites

UBM Canon | Design News | Test & Measurement World | Packaging Digest | EDN | Qmed | Pharmalive | Appliance Magazine | Powder Bulk Solids | Canon Trade Shows