I am trying to find a US supplier for PET viscosity enhancer (opaque) for extrusion applications. Something similar to Ausipol PP-30. Does anyone

Macro-M has a MacroGran Ep112

Macro-M has a MacroGran Ep112 Chain Extender that works very well and can also be purchased ia a master batch that will handle the drying temps.

Visit www.macro-M.com

BASF has their Joncryl line

BASF has their Joncryl line of chain extenders, and Clariant sells them in masterbatch form. I have tried them, they work, but can't take PET drying temperatures. Get the masterbatch for trials, ans if you need to buy/use a lot, buy the extender from BASF and mix back with powdered PET 1:10 for better distribution.
A.L. Griff algriff@griffex.com

Media Kit  |  Privacy Policy  |  Contact  |  Feedback  |  Subscribe | | |

© 2011 UBM Canon | please visit these other sites

UBM Canon | Design News | Test & Measurement World | Packaging Digest | EDN | Qmed | Pharmalive | Appliance Magazine | Powder Bulk Solids | Canon Trade Shows