surface finish, texture
By cantina88
Published: June 2nd, 2010
Published: June 2nd, 2010
Can anybody tell me where I can find specifications for mold finishes such as "SPI B-3" and "MT1140".
Thanks much,
Paul
Can anybody tell me where I can find specifications for mold finishes such as "SPI B-3" and "MT1140".
Thanks much,
Paul
Have you tried the Mold tech
Have you tried the Mold tech website? They have an excellent customer information database which provides a number of specifications for various products.
Alex
http://www.cavalok.com/
Have you tried searching the
Have you tried searching the internet for SPI B-3 and MT1140? You’ll get thousands of places where you can buy those mold finishes; you just need to look carefully. Usually mold finishes are usually pretty expensive but they are worth the money, I must say. I hope that you have found what you’ve been looking for.
Joe
http://www.litecraftcommercial.co.uk
I am sure that would have
I am sure that would have helped him find the information that he was looking for or I would just check up the web for some manufacturers and ask them to get back with the details – sure there’ll be many looking out for a deal which should work both ways!! There is so much competition going on in this field that you’ll have your pick from among them and still have a scope for bargaining!!
Regards
Burco
Mold Tech or any other
Mold Tech or any other texturing source should be happy to tell you the surface finish required for any texture that is going to be done with them. Just call them.
Generally, for any texture surface you will need to ensure that all EDM is removed. The lighter the texture, the higher the surface finish.
Mold Tech wants $450 for a
Mold Tech wants $450 for a set of texture plaques; Spendy but they'll deduct it from you first PO, the SPI plaque is $10 + freight.
Hope this helps.
Bill Tobin
I am 99% sure the MT1140 is a
I am 99% sure the MT1140 is a MOLD-TECH finish. I would contact them for a plaque. Mold-tech.com
You can buy the SPI plaque
You can buy the SPI plaque directly from SPI
Or you can order it from my website - wjtassociates.com
it should be in the 'e-bookstore'
If you can't find it on my site, e-mail me and I'll give you the link.
As to the MT1140, I don't have a clue.
Hope this helps.