TFU not ok error on battenfdeld unilog 4000 series

By futuremolding
Published: January 18th, 2011

hi all, 
   after a power interruption we are getting an error message of TFU NOT OK on my battenfeld unilog 4000 series toggle machine, hence i am unable to start t the IMM,can anyone help opn this error.
 
thanks 
 
joseph

Hello Joseph, I am also

Hello Joseph,

I am also having same problem on my since lase few days. How did you manage to get the machine running. A word from you will be of great help to me.

Thanks

Manjeet