Green Matter: Purac uses sampling strategy to promote high-performance PLA

February 26, 2013

Hoping to accelerate the market introduction of its PLA resins, Purac, the Dutch-based manufacturer of biobased chemicals and biobased monomers for bioplastics, is now offering samples of its Puralact lactide-based PLA to potential customers for testing and product evaluation purposes.

The company is approaching the market directly, offering brand owners, converters, and compounders the chance to become familiar with the resins and blends that make up the PLA portfolio. Companies interested in exploring the benefits of high-performance bioplastics can obtain test samples directly from Purac. Industrial-scale PLA product evaluations will also be supported and supplied directly by the company. For ongoing commercial quantities of PLA resins, Purac will bring interested parties in direct contact with its strategic PLA supply partners. Purac high temperature Puralact

According to Purac, "PLA is an acronym that stands for a range of different polymers." Thanks to Purac's PLA technology, the resins and blends on offer have a maximum heat resistance of up to 120°C (HDT B). This high-heat performance is achieved by improving the purity of the PLA polymer backbone. As a result, they are suitable for a wide range of applications in markets varying from consumer electronics, high-heat packaging, automotive interiors and automotive underhood components, to apparel and non-wovens.

Purac is offering three different types of PLA to interested companies for sampling and evaluation purposes. Next to its PLLA and PDLA homopolymer resins with high stereochemical purity, customers can also try out the company's PLA compounded blends. These blends are a combination of PLLA and PDLA homopolymers that have been specifically developed for injection molding and extrusion. According to Purac, their heat performance is similar to traditional PS, PP and ABS.

The PLLA is available in a range of viscosities, especially developed for cast film, thermoforming, blown film, fiber spinning, compounding and injection molding applications. Purac's PDLA homopolymer resins serve as a nucleating agent for PLLA homopolymer resins. When PDLA is combined with PLLA, the result is a compound suitable for injection molding or thermoforming that exhibits excellent heat performance and shorter processing cycle times.