Launches production programs for closures on future vehicle platforms.
December 7, 2020
After winning a JEC Innovation Award in 2016 for its Lincoln MKS Decklid Concept – a TCA Ultra Lite outer panel and a carbon fiber RTM prototype inner – Continental Structural Plastics (CSP) has fine-tuned its carbon fiber RTM (CF-RTM) process to the point that a premium automaker will be using the technology for closures on future vehicle platforms. These doors will feature both inner and outer panels as well as structural reinforcements molded using CSP’s advanced CF-RTM process.
When CSP set up its Center of Excellence for Lightweight Technologies and Carbon Fiber Processes in Pouancé, France, in 2013, the goal was to develop processes to make the use of carbon fiber in high volume applications affordable and feasible. Since then, the CSP team in Europe has been working on developing a high-performance CF-RTM process that would result in high-strength, ultra-light-weight components to help OEMs address stringent CO2 emissions regulations. Specifically, the team has been focused on improving cycle time, utilizing automated preforming and lowering the cost of the carbon fiber materials.
“We have been targeting a three-minute cycle time using 100 percent recycled carbon fiber. With our multi-material decklid concept, we demonstrated this was totally possible,” said Marc Philippe Toitgans, director, Research & Development CSP Europe. “Now we are proud to say we have collaborated with major OEMs in the United States and Europe on carbon fiber RTM programs and will see the first commercial applications of this technology very soon.”
From CAE analysis, flow simulation, preform process, mold design and full automation, CSP has built best-in-class expertise to support major structural and Class A CF-RTM programs for closures and other BIW applications. CSP’s key differentiators are based on:
100 bars of injection pressure, and up to 1,500 tonnes of pressure for closure applications
High fiber content (greater than 50%) for structural applications
20-second injection time
Management of variable thicknesses
Weight savings of up to 30% when compared to aluminum
To support several carbon fiber RTM programs that will begin as soon as the end of 2020, CSP and parent company Teijin are investing in a dedicated CF-RTM production line in Palmela, Portugal. The initial investment of €5.5 million will include the installation of compression presses, RTM injection units and a bonding cell.
“We are excited to be working hand-in-hand with our customers in Europe to demonstrate our RTM capabilities,” said Ricardo Barros, CSP/Inapal program manager. “The level of industrialization and automation we are installing in Palmela is second to none for similar carbon fiber applications.”
In addition to reducing component weight and cycle times, the CSP team in Europe has been pursuing a number of methodologies that will result in more sustainable manufacturing processes. Working toward a net zero emission target, CSP Europe is working on tomorrow’s CF-RTM process with a primary focus on natural or recycled fibers, thermoplastic/bio-sources, advanced resins, and reduced scrap and waste.
“Our goal is to keep working on a sustainable value proposition with a focus on net zero CO2 emissions,” said Philippe Bonte, president, CSP Europe. “We will achieve this via advanced manufacturing technologies and the use of renewable materials with the aim of becoming a positive contributor to the global environment.”