Polycarbonate Shines in Solar Vehicles

Image: Teijin automobile solar roof
The engineering plastic is a key enabler in range extension thanks to its light weight and transparency.

Photovoltaics is now a key enabling technology for land vehicles and boats. The favorite type is single-crystal silicon, which is even viable on the sides now. On boats, it used to be protected by an acrylic sheet on either side, making it bendable when being fitted, but this has strength and weathering issues. Now, much stronger, long-life polycarbonate is taking over, according to a report titled “Solar Vehicles 2021–2041, Second Edition” from IDTechEx.

Your car headlamps withstand being hit by a rock because of polycarbonate. Lighter than glass, it is molded into shaped panels by Sono Motors, the company with the largest solar car order book at over 10,000 vehicles partly because it is able to charge modest prices. Its solar load-bearing bodywork replaces steel and paintwork, saving that cost, yet the appearance is similarly professional. 

This year, Sono demonstrated a solar truck — again, with the solar bodywork viable even on the sides — and it landed a license deal to make the EasyMile robot shuttle solar-assisted. As private cars are banned from city centers, robot shuttles will take over, so this is the future.

Faster charging via solar

Charging is 10 to 40% faster when solar bodywork has already done some of it. This is significant because it happens with existing chargers — it is not reliant on expensive fast chargers and cars with thicker wiring. Vehicle OEMs Lightyear and Sono also take a benefit in needing less battery. That helps to address the ongoing battery supply and safety issues, smaller batteries being safer.

Teijin and its joint development partner Applied Electric Vehicles (Applied EV) have developed another polycarbonate solar roof for future mobility applications. It uses Teijin’s Panlite polycarbonate resin glazing for its surface. Teijin used its proprietary know-how in polycarbonate resin glazing and technologies to integrally mold the curved surface into an ideal vehicle shape, an extremely challenging process if using glass. Panlite achieves the strength and rigidity required for the vehicle.

Teijin’s take

Conventional polycarbonate resin offers excellent impact resistance, but it must be specially processed to realize the level of weather resistance needed for long-term outdoor use. Teijin’s Panlite glazing, however, can be given a proprietary hard coating to achieve the 10-year weather durability required for automobiles.

Teijin and Applied EV solar roof was first shown this year on the Blanc Robot, a zero-emission robotic vehicle platform developed by Applied EV using materials and technical support from Teijin. In testing conducted by Applied EV in Australia, the solar cells mounted on the Panlite roof achieved output of about 330 W, which is equivalent to a conventional solar panel housed under glass.

TeijinLS EV prototype

The zero-emission robotic vehicle platform Blanc Robot premiered the Teijin and Applied EV solar roof. Image courtesy Teijin.

Because this vehicle is light and energy efficient, the benefits of solar charging the Blanc Robot are much greater than results that could be achieved on a typical EV. Applied EV tests suggest that the solar array can contribute up to 30% of the vehicle’s energy budget in ideal conditions and around 15 to 20% on a typical day. Under the right conditions, this could extend vehicle range for the Blanc Robot by between 30 and 55 kilometers compared to the same vehicle without a Panlite roof.

Teijin and Applied EV continue to collaborate on the use of Teijin’s various material technologies in the development of further EV components, including structural elements, glazing, and exterior body panels, with the intention of commencing high-volume production in the latter half of 2022. These initiatives, together with ongoing efforts to further enhance the new solar roof, are expected to contribute to the ultimate goal of achieving Japan’s Well-to-Wheel Zero Emission policy, which calls for a 90% reduction in 2010-level greenhouse gas emissions per passenger car by 2050.

Meanwhile, Hyundai has announced that opaque and translucent solar bodywork will be widely deployed on future cars, the solar-assisted Sonata currently on sale being only a beginning. It has long collaborated with Sabic on polycarbonate vehicle glazing.

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish