Top-quality, low-haze film processed on blown line

October 1, 2005

1 Min Read
Top-quality, low-haze film processed on blown line

With the latest COEX Flex blown-film line, this equipment maker is able to achieve web clarity approaching cast film quality. Out put runs at 1.7/1.8 kg for each mm of die diameter. The unit is equipped with IBC and air cooling ring. The web has a haze value of only 4.5% on a 30-µm gauge film. The extruded three-layer film is based on a 95/40/90% metallocene linear-low-density polyethylene content. Macchi Srl, I-21040 Venegono Inferiore (VA), Italy; +39 0331 827717; www.macchi.it