Clean-Room Conveyor Is Constructed Of Stainless Steel

Clean-Room ConveyorIs Constructed OfStainless Steel


1 NPE logo 4/cAxmann Conveying Systems has introduced an all-stainless steel conveyor for use in medical and clean-room molding operations. Conveyor Type 4051 ES is producedfrom T-304L stainlesssteel and features USDA/ FDA- approved white belting, sealed bearings and optional rubber-coated rollers for wash-down applications.

Axmann ConveyingSystems, Inc.
Jeffersonville, IN 