Compounding system keeps eye on margins

EXTRUSIONThe Micro Ingredient Controller (MIC) aids rigid- and flexible-PVC processors in keeping costs in the very competitive compounding sector within pre-determined limits. According to the manufacturer, MIC provides efficient handling of materials with accuracy and repeatability that exceeds most critical requirements—standard at ±0.5% of the full-scale system deflection while minimizing adverse-impact human intervention. The E-Z Flo Fluidizing Hopper provides good material flow into the compounder. The system is a hands-off approach to compounding that minimizes labor involvement and can help maximize annual vinyl compound output. O.A. Newton, Bridgeville, DE, U.S.A.; +1 302-337-8211; www.oanewton.com