Düsseldorf — During its K 2013 press conference, Dow Chemical's elastomers group unveiled a compatibilization technology that combines both non-polar and polar polymers with polypropylene (PP).

Specifically, Dow's Intune PP-based olefin block copolymers combines polyethylene (PE), polyolefin elastomers (POE) and polar materials such as ethylene vinyl alcohol (EVOH) and polyamide (PA) with PP.