West-Coast firm Parmatech-Proform Corp. (Petaluma, CA) has acquired the metal injection molding (MIM) business of Morgan Advanced Ceramics (New Bedford, MA). The acquired business’s products are used in the medical, telecommunications, aerospace, electrical and power, semiconductor, and laser markets.

According to Peter C. Frost, president of Proform’s owner ATW Cos. (Warwick, RI), “Proform will enhance our current MIM business, expanding its MIM capabilities to the East Coast, as well as expanding production capabilities and improving product quality by leveraging ATW's expertise in precision metal components.” [email protected]