Dehumidifying dryer line expanded

Two larger models have been added to the PCT2 series of dryers, expanding the line to include eight models. The PCT2-2000 dries at rates up 2000 cfm, while the PCT2-2500 reaches 2500 cfm. Drying temperatures for the series range from 150 to 375F. Like the rest of the line the new dryers use Una-Dyn?s patent-pending Pulse Cooling Technology, as well as the FN microprocessor control, a patented Material Saver function, and return air-cooling coil.
Universal Dynamics Inc.
Woodbridge, VA
(703) 490-7001
www.unadyn.com

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish