Economical transparent nylon offers clarity, chemical resistance

Grivory GTR 45, a partially aromatic, amorphous nylon copolymer suitable for injection molding, is a transparent material that combines clarity and chemical resistance with a good balance of mechanical properties. It retains its properties after water absorption and has a 91 percent light transmission for clear applications.

According to the manufacturer, Ems-Chemie, Grivory GTR 45 compares to polycarbonate with better abrasion behavior, chemical resistance, and similar mold shrinkage. Compared to DuPont?s Zytel 330, Ems-Chemie says Grivory GTR 45 offers better clarity, toughness, elongation, and processibility, and provides shorter cycle times, lower processing temperatures, and more consistent parts. It ranges in price from $3 to $4/lb depending on quantity.

Ems-Chemie (North America) Inc.
Sumter, SC
Phone: (803) 481-6171
Fax: (803) 481-6121
http://www.emschem.com

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish