Rolls give hot film, sheet the cold shoulder

ExtrusionSheet and film processors can, together with this manufacturer, design the best solution for chill rolls to meet exact extrusion needs such as heat transfer, mechanical strength, and performance. The DuraShell chill roll series offers uniform temperature control (±0.5°C/±1°F) across the entire roll surface, performance consistency under loads up to 2100 N/cm (1200 pli), and comes in sizes ranging up to 122 cm (48 inches) diameter and 762 cm (300 inches) in length. The rolls are said to offer more resistance to worm tracking than carburized and flame-hardened shells, and they come in a variety of finish options to meet specific application needs.Xaloy, Pulaski, VA, U.S.A.; +1 540-994-2269; www.xaloy.com