IMM's Benchmarking Report: Third quarter 2000, data group 2 of 3

Article-IMM's Benchmarking Report: Third quarter 2000, data group 2 of 3

The IMM Benchmarking Report is in its third year and this month provides data from the third quarter of 2000. We've developed a strong core group of molders who have volunteered this data, but we are constantly looking for more participants. 

For those new to the Benchmarking Report, the project is simple. Several molders have volunteered to share their benchmarking data with us each quarter. The information comes in two parts. The first is the profile data (see table, below), which characterizes the molders by press quantity, resin quantity processed, parts quantity, and revenue, among other measurements. The information in the pies is the benchmarking data. We're measuring nine benchmarks: machine utilization, productive downtime, training per employee, mold change time, scheduled ship date on time, accident incident rate, scrap as produced, customer returns, and employee turnover. Each month we present three of these nine benchmarks. 

If you want to get involved, participation is easy. In return for your time and data each quarter, you get detailed reports on key production and market data for every participating molder. Anonymity is guaranteed. Contact us (see contact information below) and we'll send you the information and forms you need to get started. This service is free.





Contact information
Injection Molding Magazine
Denver, CO
Jeff Sloan
Phone: (303) 321-2322
Fax: (303) 321-3552
E-mail: 
[email protected] 
Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish