National Science Foundation Awards Grant to Rensselaer Polytechnic for Research into New Plastic

Target composed of plastic pellets
The researchers will investigate polymers with the properties of polystyrene but that can be easily depolymerized and converted into raw materials for re-use.

With the support of a $300,000 grant from the National Science Foundation, chemical engineers from Rensselaer Polytechnic Institute in Troy, NY, aim to develop a new polymer that can replace polystyrene (PS). While PS is inexpensive and easy to make, it is difficult to break down into its original components for re-use through a process called depolymerization. Founded in 1824, Rensselaer is America’s first technological research university.

“One of the problems is that polystyrene is rarely used in its pure form, which makes it harder to be re-used,” said Sangwoo Lee, an assistant professor of chemical and biological engineering, who is leading this research effort. “We aim to establish a new class of polymer that is still tough and clear but can be easily depolymerized and converted into raw materials for re-use.”

The researchers will examine potential polymers that may be suitable for use in plastic products. They will develop a library of recyclable copolymers that they will synthesize, characterize, study, and evaluate as polystyrene substitutes. Research will cover alternatives to both clear rigid PS as well as expanded polystyrene.

The team is looking for materials that will depolymerize on their own when a specific chemical is introduced. In order for such a solution to be adopted, it must be practical and affordable.

This effort builds upon a finding Lee and his team came upon as they were developing a polymer membrane to use in energy conversion. The membrane they developed kept breaking down in a systematic way, prompting Lee and his lab to explore how else it could be used. That led to this current pursuit of an economical and environmentally friendly solution to plastic re-use.

“What’s exciting about this research is that we will establish a new approach to convert used plastic into raw material,” Lee said. “It will be economical, which is one of the elements that’s missing in the process.”

Image: Hakan Tanak/Adobe Stock

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish