To cut costs associated with injection molding, prioritizing part moldability during the design phase is critical. Optimizing moldability from the outset can saves thousands of dollars.

Wall thickness is the foremost consideration in designing for moldability, according to one process expert, followed closely by optimizing ejection from the mold.

The Goldilocks principle applied to wall thickness

To avoid walls that are too fat or too thin, designing a wall thickness between 0.040 and 0.140 in. (1.0 to 3.5 mm) is ideal, according to injection molding engineer Jack Rulander of Protolabs in Maple Plain, MN. The company provides an array of digital manufacturing expertise.

“Designs that are too thick will be prone to voids/sink/high shrink, often leading to warp,” Rulander advised. “Too thin of a wall, and you will be prone to hesitation, where the melt flow slows down or stops along a particular path. This leads to cracking, weak knit lines, short shots, and more.”

To achieve optimal part ejection, he continued, engineers should add at least one degree of draft to ensure ejector pins and blades pop parts off a mold easily. Material choice plays a key role in how much draft is needed, because “semi-crystalline is often high shrink, while amorphous materials are generally low shrink. Texture and surface finish also play a role. For part ejection, undercuts and internal features may present problems and may need to be redesigned to allow successful molding.”

Consider gate vestiges

Final part appearance is another consideration for part and process design, Rulander noted. “Injection molded parts are also left with gate vestiges and witness lines from parting/shutoff surfaces. Tab gates, which are most common, offer a lot of flexibility for placement, but also can leave a larger vestige when compared to other options. For cosmetic parts, it’s important to find the ideal location where that mark is less apparent. When it comes to functional parts, these same marks or flash (excess plastic) on parting/shutoff surfaces may impact sealing.”

Optimizing mold form, fit, and function in the prototyping stage is a task ideally suited to the rapid design flexibility of 3D printing, which lets designers assess multiple part iterations before investing in costly molds for high-volume, low-cost production.

However, Rulander cautioned, “keeping the end game in mind during the prototyping stage is vital, because what works well in a 3D-printed part may not translate to injection molding. Try to design with injection molding in mind during the prototyping phase so you can quickly transition to molding larger quantities instead of going back to the drawing board.”

To avoid costly mistakes, Rulander offered these tips:

  • Start with the end in mind. “This cannot be stressed enough when it comes to saving money on your molded part. 3D printing has very few design limitations. When you try to mold a part exclusively designed for 3D printing, your best-case scenario is that the manufacturer probably had to include many costly mechanical components to the mold to accomplish it. The worst-case scenario is that it just can’t be done.”

  • Bear in mind mold-base size. “One of the largest cost drivers at Protolabs, mold-base size is not solely dependent on the size of the parts. For example, adding an undercut to a part might require a side action cam in the mold. A 1-x-1-inch part that at first required a 4-x-4-inch mold now requires a 10-x-10-inch mold, which might add thousands in tooling costs.”

  • Consider internal components. “Outside of poor part design and mold size, internal componentry is the largest cost driver. For example, cams or inserts will typically increase your overall mold price by $1,000 to $2,000 per component, so keep that in mind while you’re designing.”

Getting a ventilator to market fast

During the pandemic, Protolabs was a key advisory partner in creating Aura Project’s Aura Ventilator, a low-cost lifesaver aimed at use by nonprofits, nongovernmental organizations, and small hospitals to help underserved communities.

Protolabs provided Multi Jet Fusion 3D-printing services to Aura’s small team of developers to navigate FDA regulatory hurdles during the prototyping phase, Rulander explained.

Aura ventilator project

Protolabs produced all of the internal pieces of the Aura ventilator, as well as many of the external parts.

“While working with 3D-printed parts, the Aura team utilized Protolabs’ digital quoting platform to receive rapid quotes and DFM analysis in under an hour for injection-molded parts,” he noted. “The ability to repeatedly run accurate quotes for IM parts concurrently helped the team determine if each design change in the 3D-printed prototype would be worth the investment in the end when they moved over to IM for production parts.”

With an optimal design refined through rigorous up-front assessment, Aura transitioned into injection molding production at 500 units a month, “which equates to about 6,000 parts per month from Protolabs,” according to Rulander.

You can read the full Protolabs/Aura case study here.

About the Author(s)

Geoff Giordano

Geoff Giordano is a tech journalist with more than 30 years’ experience in all facets of publishing. He has reported extensively on the gamut of plastics manufacturing technologies and issues, including 3D printing materials and methods; injection, blow, micro and rotomolding; additives, colorants and nanomodifiers; blown and cast films; packaging; thermoforming; tooling; ancillary equipment; and the circular economy. Contact him at [email protected].

Sign up for the PlasticsToday NewsFeed newsletter.

You May Also Like