February 28, 2018

2 Min Read
BarrierPack Recyclable pouches and film support a circular economy

BarrierPack Recyclable, an innovative new polyethylene plastic laminate for premade pouches, provides positive environmental outcomes and value creation through a sustainable material with performance properties equivalent to conventional materials. It was developed in direct response to the need to reduce plastic waste without compromising on quality or functionality, and it supports a circular economy.

“Our new laminate, BarrierPack Recyclable, is a leap forward for sustainable packaging,” said Carl Stonley, Technical Account Manager at Mondi Consumer Goods Packaging. “In addition to being fully recyclable, it offers exceptional mechanical properties and is ideal for a range of packaging style formats. Constructed using two layers of PE film, BarrierPack Recyclable is a highly functional, flexible, packaging material that’s easy to open and reclose for consumer convenience. It’s functional in that the material is stiffer, stronger and lighter than a conventional PET/PE laminate of the same thickness and it can be formed directly on form-fill-seal machinery, as well as used for premade packaging.”

The moisture barrier provided by BarrierPack Recyclable makes it ideal for a wide range of applications, such as dry food, food ingredients, personal care and pet care applications.

It is currently not available in the United States. But as we've seen in the past, many European developments find their way stateside and vice versa.

ADM Cleveland 2018 showcases the latest in robotics, automation, plastics, packaging and design engineering through 5 integrated events including Pack and PLASTEC. For more information, visit the EastPack website.

New sustainable alternative

Sustainable plastic packaging is evolving faster than the general understanding of the related materials and recycling issues. Industry-wide initiatives are driving development of recyclable packaging for a circular economy that maximizes the lifecycle of plastic and minimizes its ecological footprint.

BarrierPack answers the market’s need for sustainable alternatives for flexible laminates by offering full recyclability, validated by extensive trials by CeDo Recyling in the Netherlands, a leader in recycling technologies

Ton Emans, Managing Director at CeDo Recycling & President of Plastics Recyclers Europe, said: “The European Commission announced a strategy in January 2018 to ensure that all plastics packaging is recyclable by 2030. This innovation shows that flexible plastic packaging can become truly circular. Flexible material designed for recycling is key to enabling circularity to safeguard precious resources in Europe.”

“Mondi is committed to developing sustainable plastics using circular economy design approaches, so we are delighted to be able to bring this valuable innovation to market,” Stonley added.

Mondi’s BarrierPack Recyclable laminate is debuting at the Packaging Innovations trade show in Birmingham, UK, February 28 to March 3 in Booth F19.