Compostable Corrosion-Inhibiting Stretch Film Comes to Market

Image: Cortec compostable EcoStretch
EcoStretch film from Cortec combines commercially compostable resins with Vapor phase Corrosion Inhibitor technology that imparts corrosion protection to metal molds and other equipment.

Cortec has introduced what it’s calling the “world’s first compostable corrosion-inhibiting stretch film.” EcoStretch is the next generation in a line of commercially compostable film technologies offered by Cortec, which specializes in the development of corrosion protection and packaging technologies that minimize environmental impact.

The machine-grade stretch wrap combines commercially compostable resins with Vapor phase Corrosion Inhibitor (VpCI) technology that imparts corrosion protection to multiple metal types, including aluminum, galvanized steel, carbon steel, silicon steel, stainless steel, copper, brass, and cast iron.

EcoStretch meets the ASTM D6400 standard for commercial composting and may avoid tariffs, fines, and tip fees where polyethylene is prohibited or restricted. It is suited for stretch-wrapping metal equipment such as molds and components that need to be kept rust-free while minimizing the environmental impact of traditional plastic packaging.

Corteccompostability day one

Corteccompostability week three

Corteccompostability week six

EcoStretch compostability (left to right) on day one, week three, and week six.

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish