Innovia Films introduces crystal clear in-mold label film

Innova Films crystal clear IML film
A crystal clear in-mold label film from Innovia Films Ltd. (Cumbria, UK) produced using a “unique bubble process” debuts.

Crystal clear cans and containers for food are the new reveal in packaging, showing “clearly” what’s inside. To accommodate the clear cans and containers, and meet managers’ new focus in helping their products succeed in a demanding market environment, Innovia Films Ltd. (Cumbria, UK) announced a new crystal clear in-mold label (IML) film produced using the company’s “unique bubble process.”

The exceptional clarity of RayoForm ICU is unprecedented in the industry, boasts Innovia Films, “making it the clear leader to showcase brands and their products.”

Richard Southward, Global Product Manager, Labels explains, “There is a continued trend toward clear containers. Brand managers favor them because they allow consumers to see the nature, quality and color of their products before purchase. Clear containers also allow brands to enhance their on-pack branding efforts and offer greater shelf impact.”

RayoForm ICU has been specifically developed to maximize brand impact by the use of clear containers. It also maximizes printing and molding performance and efficiencies. Print trials have shown ICU can readily exceed industry standards for sheets per hour. The films’ balanced mechanical properties offer potential SKU reduction as sheets can be sheet-fed in multiple directions. For the molder, RayoForm ICU offers increased productivity through faster label handling, enhanced container shape retention and more efficient stacking, Innovia said.

“RayoForm ICU is currently available in thickness of 58 micron/230 gauge,” said Southward. “We are already seeing a lot of interest in this new product and are happy to provide trial reels to prove its excellent performance.”

Innovia Films is a major producer of highly differentiated specialty biaxially oriented polypropylene (BOPP) films using a proprietary ‘bubble’ manufacturing process. With global production sites in Australia, Belgium and the UK, Innovia has a “leading position” in the markets for high performance coated films, tobacco overwrap, labels and security films. With a workforce of 850 worldwide, the company is focused on high quality value added products, strong customer relationships, R&D and excellent service, according to Innovia.

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish