World’s First 100% Enzyme-Recycled PET Plastic Bottles Debut

Jerome Palle Bottles-Consortium-Group-Photo-Jerome-Palle-FTR.jpg
PET recycling breakthrough from Carbios, L’Oréal, Nestlé Waters, PepsiCo and Suntory Beverage & Food Europe yields food-grade PET bottles.

The promise of endlessly recycled PET plastic is one step closer as the Consortium of Carbios, L’Oréal, Nestlé Waters, PepsiCo and Suntory Beverage & Food Europe announced the successful production of the world’s first food-grade PET plastic bottles produced entirely from enzymatically recycled plastic.

Each Consortium company has successfully manufactured sample bottles based on Carbios’ enzymatic PET recycling technology for some of their leading products including: Biotherm, Perrier, Pepsi Max and Orangina.

It’s the culmination of nearly 10 years’ research and development by Carbios to create a new process and supercharge an enzyme naturally occurring in compost heaps that normally breaks down leaf membranes of dead plants. By adapting this enzyme, Carbios has fine-tuned the technology and optimized this enzyme to break down any kind of PET plastic (regardless of color or complexity) into its building blocks, which can then be turned back into like-new, virgin-quality plastic.

Carbios’ patented enzymatic PET recycling process enables a wide variety of PET plastics to be recycled into virgin quality, food grade rPET. PET plastics that would otherwise go to waste or be incinerated, can now be brought back into a continuous circular system of recycling. And this can be achieved at high speed — breaking down 97% of plastic in just 16 hours. That’s 10,000 times more efficient than any biological plastic recycling trial to date (peer-reviewed article in Nature).

CarbiosCarbios-Enzyme-Explainer-Infographic-Art.jpg

Together, these brands will work to scale this innovation to help meet the global demand for sustainable packaging solutions. In September 2021, Carbios will break ground on a demonstration plant, before launching a 40,000 tons capacity industrial facility, by 2025.

Enzymatic recycling overcomes the issue of degradation in conventional recycling and can be used on any type of PET plastic. Because Carbios’ recycling process works under mild conditions, it could also lower the carbon footprint of PET waste treatment by saving 30% of CO2 emissions compared to a conventional end of life mix of incineration and landfill, taking virgin PET production substitution into account.***

The successful completion of these initial food-grade bottles is a major milestone in the Consortium’s validation of Carbios’ technology. This partnership is part of a growing trend amongst brands to collaborate across industries to tackle these global challenges, working towards a world of circularity, where we limit the production of virgin plastic.

Carbios will license its technology to PET manufacturers worldwide, accelerating the global adoption of enzymatic recycling for all kinds of PET based products.

CarbiosCARBIOS_VERTI_Baseline-logo-Art.jpg

Members comment.

 “This is a truly transformational innovation that could final fully close the loop on PET plastic supply globally, so that it never becomes waste.” – Carbios’ CEO Jean Claude Lumaret

“We have been working with Carbios since 2017 to develop this first bottle made from PET derived from enzymatic recycling technology, an alternative to mechanical recycling. We are pleased to announce today the feasibility of these bottles in a pilot phase and are delighted to be in a position to create the packaging of the future with our partners. This is a promising innovation for the years to come that demonstrates our commitment to bring to market more environmentally friendly packaging and which is part of a circularity initiative begun more than 15 years ago” — Jacques Playe, L’Oréal’s Global Head of Packaging and Product Development added: 

 “It is very exciting to see that the quality of the prototype bottles made from colored recycled PET materials is virtually identical to clear virgin PET. When we reach industrial scale, this enzymatic recycling technology will enable us to produce high-quality rPET bottles and help Nestlé Waters in our journey to boost the circular economy and reduce the use of virgin plastics.” — Jean-Francois Briois, Head of Packaging Material Science and Environmental Sustainability Nestlé Waters global R&D

 “PepsiCo is committed to building a circular economy to achieve our vision that packaging never becomes waste. We are dedicated to reducing the virgin plastic we use and with the breakthrough Carbios enzymatic recycling technology, we can help keep valuable material in the circular economy, reduce waste and take another step toward a truly closed loop system.” — Ron Khan, Global VP of Packaging, Beverages, PepsiCo.

 “The global issue of plastic waste requires transformational thinking, creative partnerships and innovative brands coming together to seek out new solutions. Continued investment in new ways of tackling waste and creating true circularity such as this ground-breaking technology from Carbios will be key to Suntory Beverage & Food Europe achieving its 100% sustainable plastic ambition.” — Roberto Vanin, Chief R&D Officer, Suntory Beverage & Food Europe. 

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish