PC Film Reduces Gloss, Protects Against Scratches

Makrofol DE 7- CG is a graphics-arts-quality polycarbonate film said to provide excellent scratch resistance and a low-gloss look. Suitable for applications such as automotive-interior flat appliques, it has a velvet first-surface and a fine matte second-surface, with a specification range of 3.0 to 4.0 inked gloss on the velvet surface. The film comes in thicknesses of 0.015 and 0.020 in. Bayer, 100 Bayer Rd., Pittsburgh, PA 15205 www.BayerPlastics.com