Compatibilizers for pp alloys

Interloy P1085H1 PP/PS graft copolymer improves compatibility of PP with SEBS, producing very high-impact blends. It is also effective for alloying PP with Noryl and other polyphenylene ether/PS blends. Grade W1095H1, a PP/acrylic graft copolymer, improves gloss, weatherability, and mar resistance in acrylics, polycarbonate, and ABS for outdoor and automotive applications. Crompton Corp., Benson Rd., Middleburry, CT 06749, www.cromptoncorp.com