Three new flexible vinyl compounds for molded and extruded exterior automotive applications have received approval under Ford global specification WSK-M4D689, according to material supplier Teknor Apex (www.teknorapex.com). Materials include Apex 72B-427D-21D (80 Shore A), Apex 1523F (75 Shore A), and Apex 1523E-8 (65 Shore A), and can be found in window encapsulation, body side strips, and trim components in 2008 Ford cars, SUVs, and trucks. Shown is a window encapsulation.