Düsseldorf - Solvay Acetow is announcing the introduction of its new Ocalio cellulose acetate bio-plastic, manufactured using wood pulp, for the first time here at the K show. "Actually, what people mostly know about us is that 95% of our material is used to make cigarette filters," said Louis Cozzari, Business Development Manager at Solvay Acetow. "But now we're diversifying into other products. We are, after all, a natural based, "green" material. We source all our wood pulp from SFI certified forests. So, with our material, there is no competition with food."

October 19, 2013

1 Min Read
It's new and it's green from Solvay Acetow: cellulose acetate bioplastic

Düsseldorf - Solvay Acetow is announcing the introduction of its new Ocalio cellulose acetate bio-plastic, manufactured using wood pulp, for the first time here at the K show. "Actually, what people mostly know about us is that 95% of our material is used to make cigarette filters," said Louis Cozzari, Business Development Manager at Solvay Acetow. "But now we're diversifying into other products. We are, after all, a natural based, "green" material. We source all our wood pulp from SFI certified forests. So, with our material, there is no competition with food."

Click here to read the entire article on PlasticsToday.

Sign up for the PlasticsToday NewsFeed newsletter.

You May Also Like