Zero-halogen fr foam

Zotefoams is developing a nonhalogenated, closed-cell, crosslinked, polyolefin flame-retardant foam that conforms to U.S. automotive standards and UL94-HF1. Samples are available of a 24kg/cu m density foam that complies with FMVSS.302 at 2 mm. The new materials will be commercially available in a 2000-by-1000-by-30-mm sheet size. Zotefoams Plc, 675 Mitcham Road, Croydon CR9 3AL England www.zotefoams.com