Washington State University team develops promising means of recycling carbon-fiber thermoset plastic composites

Carbon fiber reinforced plastics are increasingly popular in many industries, particularly aviation, because they are light and strong. They are, however, very difficult to break down or recycle, and disposing of them has become of increasing concern. While thermoplastics can be melted and recycled relatively easily, most composites used in aerospace are thermosets, which present challenges for reuse.

Jinwen Zhang with his carbon fiber recycling research team

To recycle thermoset carbon fiber composites, researchers have generally tried grinding them down mechanically or breaking them down with very high temperatures or harsh chemicals to recover the expensive carbon fiber. Oftentimes, however, the carbon fiber is damaged in the process. The caustic chemicals used are hazardous and difficult to dispose of. They also destroy the matrix resin materials in the composites, creating a messy mixture of chemicals and an additional waste problem.

In their project, Jinwen Zhang, a professor in the School of Mechanical and Materials Engineering, and his team developed a new chemical recycling method that used mild acids as catalysts in liquid ethanol at a relatively low temperature to break down the thermosets. In particular, it was the combination of chemicals that proved effective, said Zhang, who has a chemistry background. To break down cured materials effectively, the researchers raised the temperature of the material so that the catalyst-containing liquid can penetrate into the composite and break down the complex structure. Zhang used ethanol to make the resins expand and zinc chloride to break down critical carbon-nitrogen bonds.

“It is critical to develop efficient catalytic systems that are capable of permeating into the cured resins and breaking down the chemical bonds of cured resins,” he said. The researchers were able to preserve the carbon fibers as well as the resin material in a useful form that could be easily re-used. They have filed for a patent and are working to commercialize their methods.

The work was funded by the Joint Center for Aerospace Technology Innovation (JCATI) in collaboration with industry partner, Global Fiberglass Solutions. The state-funded JCATI works to support the Washington’s aerospace industry by pursuing research that is relevant to aerospace companies and by providing industry-focused research opportunities.

In addition to Zhang, researchers on the project included Junna Xin, assistant research professor, Tuan Liu, postdoctoral research associate, and graduate student Xiaolong Guo. The research is in keeping with WSU’s Grand Challenges initiative stimulating research to address some of society’s most complex issues. It is particularly relevant to the challenge of “Smart Systems” and its theme of foundational and emergent materials.