(Rockaway, NJ). The additives create a microcellular structure (cells less than 100 µm in size) via a chemical reaction that releases a small volume of gas, producing a cellular structure at a size unachievable with present-day chemical foaming agent (CFA) technology. This will expand the polymer by up to twice its volume.
Ecocell can be used with low- and high-density polyethylene, copolymer polyethylenes, polypropylene homopolymers and copolymers, crystal and impact polystyrene, PVDF, TPOs, and TPEs. It is intended for use in such applications as injection molding, thermoforming, sheet, structural foam molded parts, oriented polypropylene films, foamed label stock, blowmolding, extruded profiles, and plastic lumber. —immeditoria[email protected]