Ships Combines Gloss, Toughness, Processability

Avantra 594E is a super-high-impact polystyrene that boasts superior gloss as well as high-flow characteristics not typically available in ships. It also reportedly provides better corner and surface impact strength in finished parts, as well as processing flexibility because impact strength remains stable over a wide range of conditions. BASF, 3000 Continental Dr. N., Mt. Olive, NJ 07828 www.basf.com/plastics