Schoeller Allibert submitted a crate equipped with a moveable partition. This enables the fully automated packing of multi-packs in the crate, as the partition is pushed down at moment of filling. When the crate is unpacked at the retailer's, the partition automatically moves up, ready to be filled with empty bottles being returned to the brewery and fully protecting the empty bottles against breakage. This crate meets the demands of the market for smaller packaging for returnable bottles. The crate can be used as a point of sales display. The crate is made of foamed polypropylene, to get the right stacking strength; the stainless steel spring maintains functionality during product lifetime. The in-mold label cannot be polluted with stickers, because these do not stick on the label - this ensures that the branding is always clean at point of sales.