Bio-based innovation award finalists announced

Bio-based material of the year award

The 12th annual International Conference on Bio-based Materials will be coming soon to Cologne, Germany, and one highlight of the event is the presentation of the innovation awards. Twenty-one applications were whittled down to six finalists, which are described here. The products range from sanitary pads, which are classified as a medical device by FDA, to home-compostable coffee capsules that are said to outperform deep-drawn PP EVOH multilayer capsules. At the conference on May 15 and 16, the three winners will be announced.

The event is organized by nova institute (Hürth, Germany), an independent research organization focused on a bio-based economy. More information about the conference is available on the organization’s website.

Here are the six finalists in alphabetical order.

Aakar Innovations (Navi Mumbai, India): Anandi Eco+ 100% compostable sanitary pads

Aakar bio-based sanitary padsAnandi Eco+ is the only government-sanctioned lab-certified 100% compostable sanitary pad on the Indian market, according to the company. In a compost environment, at least 90% of the pad biodegrades within 180 days. The biodegradation process takes longer under other environmental conditions.

Aakar said that it uses local resources like jute, bagasse, banana fiber and water hyacinth to produce the sanitary pads. No harmful chemicals are used, and the resulting composted material is suitable for further use.

The product complies with compostability and labelling standards ASTM D6400 and EN 13432.

 

Carbiolice (Riom, France): Evanesto Zero-Impact PLAstic

CarbioliceCarbiolice reports that it has developed a disruptive technology that uses enzymes to speed up the compostability and biodegradability of PLA. Developed as an additive, Evanesto can be used with conventional plastics transforming processes without modifications. The additive is best suited for applications involving single-use plastics, where compostability and biodegradability are a meaningful end-of-life solution, according to the company. It can be used to make products that are 100% compostable and biodegradable.

The technology has been successfully demonstrated on thin films and sheets through tests performed by Organic Waste Systems N.V. under domestic composting conditions according to NF T51-800.

The company plans to bring Evanesto to market in early 2020.

 

Golden Compound (Ladbergen, Germany): HOMEcap home compostable coffee capsules

Golden Compound HomeCapHOMEcap is described as the world's only capsule that has been certified to the OK compost HOME standard by TÜV Austria. It is made from a unique compound comprising PTTMCC’s PBS and PBSA mixed with sunflower seed shells and inorganic fillers. A cellulose-based lid seals to the capsule without glue and is home compostable, as well.

The material composition results in low oxygen transmission rates, eliminating the need for additional barrier packaging.

A VDI 4605 sustainability assessment showed that the capsule outperforms current state-of-the-art capsules such as deep-drawn PP EVOH multilayer products.