The Heavy Gauge Value Add Silver Award at the SPE Thermoforming Conference Parts Competition went to Kintz Plastics (Howes Cave, NY).The top cover for the medical laser unit, made of Kydex-T (acrylic/PVC), measures 20 x 34 in. The sidewalls had zero draft and horizontal ribbing for venting, undercuts and numerous recesses.To view the next slide, click on the arrow under the image.

Clare Goldsberry

September 16, 2015

1 Min Read
SPE thermoforming competition: And the winners in the Heavy Gauge category are--Kintz Plastics

The Heavy Gauge Value Add Silver Award at the SPE Thermoforming Conference Parts Competition went to Kintz Plastics (Howes Cave, NY).

The top cover for the medical laser unit, made of Kydex-T (acrylic/PVC), measures 20 x 34 in. The sidewalls had zero draft and horizontal ribbing for venting, undercuts and numerous recesses.

To view the next slide, click on the arrow under the image.

kintz_0.JPG

About the Author(s)

Clare Goldsberry

Until she retired in September 2021, Clare Goldsberry reported on the plastics industry for more than 30 years. In addition to the 10,000+ articles she has written, by her own estimation, she is the author of several books, including The Business of Injection Molding: How to succeed as a custom molder and Purchasing Injection Molds: A buyers guide. Goldsberry is a member of the Plastics Pioneers Association. She reflected on her long career in "Time to Say Good-Bye."

Sign up for the PlasticsToday NewsFeed newsletter.

You May Also Like