Visual inspection system for medical applications
August 23, 2008
1 Min Read
A high-resolution X-ray visual inspection system was developed for noncontact, nondestructive inspection of products in the medical device and pharmaceutical packaging industries. Porosity and voids are inspected in low-density plastics, ceramics, and composites. The system features 7X to 45X magnification and simultaneous dual-monitor X-ray and color video image, and detects deformations and defects as small as .01 mm.
Glenbrook Technologies
Randolph, NJ
(973) 361-8866
www.glenbrooktech.com