The HD-BOPE technology reportedly allows converters to make recyclable multi-layer films that perform as well as traditional mixed-material structures.

Clare Goldsberry

July 1, 2020

2 Min Read
Nova Chemicals’ Biaxially Oriented PE Film Technology Achieves Milestone in Recyclability

Recycling multi-material barrier film packaging has been challenging producers of this type of packaging in spite of the tremendous benefits in shelf stability and longevity that barrier films bring to food packaging. Nova Chemicals Corp. believes it has a solution. On June 30, the company headquartered in Calgary announced the development of high-density resin technology for the biaxially oriented polyethylene (BOPE) market. HD-BOPE is a transformative technology that enables the manufacture of all-polyethylene, recyclable multi-layer film structures with significantly improved physical performance versus blown film, said Nova Chemicals. The technology is seen as ideal for use in food packaging, heavy duty sacks, e-commerce, and other demanding applications.

HD-BOPE resins are designed for use in the print web and can then be laminated to a sealant film made with lower-density polyethylene.

The development of this technology marks a major advance in the pursuit of a circular economy for plastics, according to Nova Chemicals. HD-BOPE can enable film manufacturers to realize fully recyclable PE mono-material structures without sacrificing stiffness or print clarity. Mono-material film structures are critical to achieving brand owner commitments to make all plastic packaging 100% recyclable, reusable, or compostable.

“Brand owners and consumers are looking for easy-to-recycle packaging that prevents contamination and extends the shelf life of their products,” said Alan Schrob, Consumer and Industrial Films Group Manager in Nova Chemicals’ polyethylene business. “Our HD-BOPE technology provides an additional building block for converters to make recyclable multi-layer films that perform as well as traditional mixed-material structures.”

Biaxially oriented films are stretched in both the machine and transverse direction, resulting in films that have enhanced toughness, barrier performance, and optics. Film structures that use the technology are commonly laminates; HD-BOPE resins are designed for use in the print web and can then be laminated to a sealant film made with lower-density polyethylene. The finished film also has high stiffness, which enables down-gauging and improved processability in converting steps versus blown film alternatives. Its low tear properties support easy-open packaging. Similar to films made from other biaxially-oriented technologies, BOPE films demonstrate excellent thickness uniformity and film flatness for high yield rates, explained Nova.

Nova Chemicals has been working with Brückner Maschinenbau, a global stretching line manufacturer, to accelerate the development and commercialization of the technology. “We have been very pleased with the performance of Nova Chemicals’ products on our equipment and are getting positive feedback from the converters who are making film with it, as well,” said Sebastian Ruhland, Senior Sales Manager, Brückner Maschinenbau. “We believe this technology will open completely new possibilities to provide PE films for 100% mono-material packaging films as an answer to the recyclability challenges we’re facing.”

About the Author

Clare Goldsberry

Until she retired in September 2021, Clare Goldsberry reported on the plastics industry for more than 30 years. In addition to the 10,000+ articles she has written, by her own estimation, she is the author of several books, including The Business of Injection Molding: How to succeed as a custom molder and Purchasing Injection Molds: A buyers guide. Goldsberry is a member of the Plastics Pioneers Association. She reflected on her long career in "Time to Say Good-Bye."