University of East Anglia researcher Aram Saeed holding 3D-printed IOL-like device
Medical3D-printed Lens Implant Could Revolutionize Cataract Surgery3D-printed Lens Implant Could Revolutionize Cataract Surgery
A polymer blend developed by academic researchers coupled with stereolithography has the potential to accelerate the design and manufacture of intraocular lens implants.