TPE Portfolio Targets E-mobility Market

Durable design of vehicle interiors for new utilization concepts such as car sharing, and more effective reduction of driving noise due to quieter electric drives are boosting demand for thermoplastic elastomers in electric vehicles.

Stephen Moore

March 4, 2020

3 Min Read
TPE Portfolio Targets E-mobility Market

With its broad range of thermoplastic elastomers (TPEs) and specific focus on the trends and challenges of electromobility, Kraiburg TPE says it is in a good position to support OEMs and system suppliers in advancing decisive innovations in this fast-growing market segment.

Kraiburg TPE is focusing on the new mobility market – including e- mobility – with a broad range of thermoplastic elastomers. (Image: © 2019 Kraiburg TPE)

For many years, TPEs have been used frequently for exterior and interior applications, as well as applications for engine compartments and power trains of motor vehicles. Although the requirements in the specific field of e-mobility are different in some respects, they are an advantage for the extremely adaptable property profile of TPEs.

According to Michael Pollmann, Director Sales & Marketing EMEA at Kraiburg TPE, important trends include durable design of vehicle interiors for new utilization concepts such as car-sharing, as well as more effective reduction of driving noise due to quieter electric drives, and good adhesion to technical plastics, such as polyamides, for two-component injection molding.

“In addition, there is a strong trend towards lightweight design to reduce the energy consumption of electric vehicles,” Pollmann says. “Other requirements include enhanced thermal conductivity and flame retardancy. We are striving to coordinate the specifications for each application with OEMs and tier 1 customers as early as possible. In the process, we are using our specific experience from other application areas such as electrical engineering and electronics to accelerate the development, release, and launch of applications.”

Typical examples can be found over the entire range of e-mobility solutions, from two-wheelers through to commercial and off-road vehicles. Electric drives, as well as autonomous and connected vehicles, also mean the integration of more and more electronic and sensor systems into vehicles. System integrity requires materials solutions that provide reliable heat dissipation, hermetic sealing, and shock absorption.

Special TPEs with a very low compression set, therefore, provide the perfect properties for durable housing seals made of cost-efficient two-component moldings with other materials, including polar thermoplastics. Integrated two-component applications with TPE can also have a significant additional noise-reducing effect. This is particularly important, as creaking and squeaking noises caused by individual components rubbing against each other are a much greater nuisance due to the quieter drive of electric vehicles.

In addition, Thermolast compounds from Kraiburg TPE are characterized by excellent flowability and are thus suitable for thin-walled soft-touch surfaces, while precisely matching even the most complex tool contours. Kraiburg TPE also has advanced development and laboratory capacities for material development and customer support, enabling the company to exactly adjust the desired property profile in terms of texture, adhesion, color, wear and scratch resistance, flame retardancy, low VOC, and odor emission, among other attributes, to each application.

In addition, all Kraiburg TPE materials are produced in accordance with the same quality standards worldwide. “That’s why we not only have the necessary expertise in custom-engineered TPEs for e-mobility applications but are also capable of effectively supporting the projects of global OEMs and suppliers from Germany to China in this booming market segment,” emphasizes Pollmann.

About the Author(s)

Stephen Moore

Stephen has been with PlasticsToday and its preceding publications Modern Plastics and Injection Molding since 1992, throughout this time based in the Asia Pacific region, including stints in Japan, Australia, and his current location Singapore. His current beat focuses on automotive. Stephen is an avid folding bicycle rider, often taking his bike on overseas business trips, and a proud dachshund owner.