PAEK materials being optimized for laser sintering
The UK’s University of Exeter commissions recently launched AM (3D printing) platform as part of its ongoing collaboration with Victrex to optimize the advantages of PAEK polymers.
January 10, 2020
The University of Exeter, in collaboration with Victrex, has completed commissioning of an EOS P 810 laser sintering platform for high temperature polymers. The strategic arrangement aims to introduce next-generation Victrex PAEK polymers and composites while improving the performance of the underlying AM (additive manufacturing) processes. Investment in the new state-of-the-art equipment, and its commissioning, are expected to accelerate the commercialization of AM materials for high performance parts.
High-temperature PAEK polymers can be printed on the EOS P 810 laser sintering platform. Image courtesy of Victrex. |
The Centre for Additive Layer Manufacturing (CALM) at Exeter is one of the first to commission the recently launched equipment. “We can now further our research by utilizing the next generation of high temperature systems, the EOS P 810,” explains Professor Oana Ghita, the lead of CALM at the University of Exeter. “The new equipment allows us to link the fundamental research with the commercial manufacturing process, to optimize the materials and their application, while accounting for the new thermal, optical, and mechanical upgrades and providing us with accurate insights into the detailed dynamics of laser sintering.”
The new EOS P 810 is capable of printing with materials that have melting temperatures around 300°C (572°F) and particularly suitable for the new low-melting-point PAEK polymers, designed and optimized by Victrex specifically for AM. The work invested in this production-ready machine, which has a build volume of 700 x 380 x 380 mm (2.30 x 1.25 x 1.25 ft) and two 70-Watt lasers, is aimed at ensuring that future demand for large-scale parts will be readily met by the market as the platform is rolled out across the supply chain.
Victrex Director of Innovation, Ian Smith, added “This is an exciting milestone in our collaboration with the University of Exeter, which we announced in 2018, creating an effective eco-system to accelerate the commercialization of AM materials for performance parts to meet customer needs.”