Lignin Additive Boosts Properties of Carbon Fiber, Recyclable Plastics
Chemically altered lignin combined with polyacrylonitrile strengthens carbon fiber while making it even lighter in weight.
August 20, 2022
The second most abundant biopolymer on Earth, lignin has understandably captured the interest of researchers over the years as a potential renewable component of polymers. The most recent innovation comes from Washington University in St. Louis, where lignin-related research may lead to even stronger, lighter carbon fiber as well as plastics with a smaller environmental footprint.
Lignin provides rigidity and structure to plant tissues, but until recently it was largely considered industrial waste beyond its botanical function. That is changing. Back in 2016, the first commercial-scale plant to extract lignin was built in Alberta, Canada, with the goal of replacing fossil-fuel sourced petrochemicals. More recently, a research consortium in Japan developed thermoset composite materials that incorporate lignin in automotive components.
The research at Washington University involves chemically altering lignin so that it can be used as a precursor for an enhanced form of carbon fiber. It reportedly could also enable the development of recyclable plastics with improved properties. By altering some of lignin’s properties, Joshua Yuan, professor and chair of the Department of Energy, Environmental & Chemical Engineering, and his team created High Molecular Weight Esterified Linkage Lignin (HiMWELL). They combined it with polyacrylonitrile (PAN) to formulate the precursor.
Yuan’s previous research identified the main roadblocks that would compromise the integration of lignin in this type of material:
The non-uniformity of lignin’s chemical structure and its molecular weight, making it difficult to combine with other polymers;
its high number of OH groups, a reactive pairing of oxygen and hydrogen that attracts water, which is not ideal for building a rigid material like carbon fiber.
To skirt those roadblocks, Yuan and his team redesigned lignin structures.
When combined with PAN, the HiMWELL-based carbon fiber had a record tensile strength and showed better mechanical properties than standard carbon fiber, reports Brandie Jefferson on the university’s newsroom page. “When it was added to recyclable polymer blends, HiMWELL improved mechanical properties and also improved UV protection,” said Jefferson.
This research lays the groundwork for using lignin in carbon fiber, according to Yuan, while diverting a material from the waste stream. The research was published in Cell Press Matter.