This line of custom engineered mold components features diameter tolerances smaller than have previously been available. Rosspunch miniature stainless steel mold components are available with multidiameter details ranging from .02 to 1 inch with diameter tolerances of ±.0001 inch. The components are precision ground from either 300 or 400 Series stainless steel and can be manufactured to customer specifications. They?re produced with custom head styles and precision-ground ends incorporating radiuses, flats, and odd shapes. They can be made in custom lengths up to 8 inches with a ±.0005-inch tolerance.