Detecting packaging defects

July 1, 2008

1 Min Read
Detecting packaging defects

AUXILIARIES

Food packaging films need to provide the highest material quality both in packaging integrity and surface printing. Automated visual inspection systems are used in individual processing steps such as extrusion, calendering, coating, laminating, cutting, wrapping, and printing to ensure defects don’t enter the distribution stream. This producer’s high-resolution camera systems can catch fisheyes, blacks specs, impurities, or holes during production of transparent, dyed, or translucent films, as well as during packaging of fluid products to guarantee protection against leakage. Product documentation from start to finish is possible with these inspection systems using the integrated SQL database.ISRA Vision AG, Darmstadt, Germany; +49 6151-948-0; www.isravision.com