Portable gloss meters now come equipped with Bluetooth for transmission of measurements on the go. The micro-gloss family from BYK-Gardner (Columbia, MD) also feature improved continuous and difference modes and transfer data with a USB cable interface or wireless with Bluetooth. An automatic check of the calibration standard ensures long-term, stable calibration. The measurement range is up to 2000 gloss units. Data is also temperature stable, and Easy-link software is provided for direct data transfer to Excel.

IMM Staff

March 3, 2010

1 Min Read
Wireless gloss transmission

(Columbia, MD) also feature improved continuous and difference modes and transfer data with a USB cable interface or wireless with Bluetooth. An automatic check of the calibration standard ensures long-term, stable calibration. The measurement range is up to 2000 gloss units. Data is also temperature stable, and Easy-link software is provided for direct data transfer to Excel. —[email protected]