Recycling of rigid plastics rose to one billion pounds in 2012

The recycling of rigid plastics excluding bottles rose to nearly 1.02 billion pounds in 2012, an increase of 10 percent over 2011 and triple the amount recycled in 2007 when the industry first began tracking rigid plastics recycling.

The "2012 National Report on Postconsumer Non-Bottle Rigid Plastic Recycling" attributes the 82 million-pound increase to the growth in the collection of plastics beyond bottles in municipalities across the U.S.

"Tripling the recycling rate for rigid plastics in just six years is an amazing accomplishment," said Steve Alexander, executive director of the Association of Postconsumer Plastics Recyclers (APR). "In a short period of time, rigids have become the fastest growing category of plastics recycling, and we're excited about the future."

Approximately 57 percent of the rigid plastics collected was processed in the U.S. and Canada with the remainder exported, primarily to China. Recycling statistics in 2012 were not affected by China's "Green Fence" policy, which began in February 2013. 

Polypropylene and polyethylene plastics comprise the largest portion (72 percent) of postconsumer rigid plastics collected in the United States with polypropylene constituting 38 percent of all rigid plastics recycled and high-density polyethylene constituting 34 percent. According to the report, polypropylene and polyethylene generally have the highest market value in both domestic and export markets because they are relatively easy to process and have a wide range of manufacturing uses.

"We are thrilled to see this kind of growth in rigid plastics recycling," said Steve Russell, vice president of plastics for the American Chemistry Council. "The increasing popularity of large bins and access to single-stream collection programs are making it easy for consumers to recycle their used plastics. We look forward to continuing to work with APR and other stakeholders in the ongoing effort to recycle and recover more plastics."

Primary domestic end uses for recycled rigid plastics include crates, buckets, pipe, auto parts, and lawn and garden products.  Consumer products such as cutting boards, food storage containers and other types of kitchenware are becoming popular end uses, as are toothbrushes and razors. A small portion of recycled rigid plastics is used in composite materials for products such as outdoor lumber, pallets and railroad ties.

This is the sixth annual report on rigid plastics recycling conducted by Moore Recycling Associates and commissioned by the American Chemistry Council's Plastics Division.

The report - and the survey on which it is based - defines non-bottle rigid plastics to include two major categories: containers (packaging and non-packaging) and bulky items.  Containers include items such as blister packs, cups, tubs, trays, clamshells, caps and lids. Bulky rigids include items such as carts, crates, buckets, toys and lawn furniture.

A separate report, also conducted by Moore Recycling Associates, has determined that over 60 percent of Americans have local access to a recycling program that collects rigid plastics.

Recycling statistics for plastic bottles and flexible plastic wraps and bags, also known as "film," are collected through the same survey and each category is reported separately.

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish