Automotive & MobilityPP Compound First to Receive UL Certification for Thermal Runaway Protection of EV BatteriesPP Compound First to Receive UL Certification for Thermal Runaway Protection of EV Batteries
Sabic’s Stamax 30YH570 resin is reportedly the first polymer to earn a UL Verified Mark, conforming to the UL 2596 thermal runaway box test.