Material handling hose withstands abrasion

A new thermoplastic urethane material handling hose with external wear strip has good resistance to abrasion and repels oils, fuels, and other chemicals. Called the Super Flow SF-TPUMH, this flexible clear hose contains copper wire for static grounding and has a smooth interior for optimum flow. It is durable with a high tensile and tear strength and can handle temperatures from -65F to 200F. The hose is also halogen-free and resists ozone, weather, and fungus. Standard lengths are 25 or 50 ft with diameters ranging from 1 to 10 inches. Price was not given.

U-Nova Hose Corp.
Richmond Hill, ON
Phone: (905) 731-9411
Fax: (905) 731-7086
http://www.u-nova.com