Medical plastics compounder and processor Biomerics used this week's Medical Device & Manufacturing show in New York, June 7-9 to announce the launch of its Quadrathane family of polycarbonate-based thermoplastic polyurethane for the medical device market. The materials are foreseen especially for use in implantable devices.
PlasticsToday Staff
June 8, 2011
1 Min Read
Medical plastics compounder and processor Biomerics used this week's Medical Device & Manufacturing show in New York, June 7-9 to announce the launch of its Quadrathane family of polycarbonate-based thermoplastic polyurethane for the medical device market. The materials are foreseen especially for use in implantable devices.