Bioplastic may replace plasticizers in PVC IV tubing

New biobased PHA (polyhydroxyalkanoate) copolymers can replace plasticizers in polyvinyl chloride (PVC), potentially enhancing its acceptability in the medical market.Metabolix (Cambridge, MA) says it has demonstrated that a series of PHA copolymers miscible with PVC resins improved various physical properties.  PHA copolymers, for example, performed as high molecular weight, readily dispersible plasticizers, enabling formulation of compounds with low additive migration and low extractables.

October 23, 2012

3 Min Read
Bioplastic may replace plasticizers in PVC IV tubing

Metabolix (Cambridge, MA) says it has demonstrated that a series of PHA copolymers miscible with PVC resins improved various physical properties.  PHA copolymers, for example, performed as high molecular weight, readily dispersible plasticizers, enabling formulation of compounds with low additive migration and low extractables.

That's a key issue for IV bags and tubing where some major hospital systems, such as Kaiser Permanente, are moving away from PVC because of concerns about plasticizer leaching.

PHAs from Metabolix are produced in a biological fermentation process using agricultural feedstocks, such as sugars derived from corn. They have been used in a variety of biomedical applications such as sutures and surgical meshes and are biocompatible. Metabolix is working on genetic engineering technology to produce PHAs directly in plant crops such as switchgrass and sugarcane.

Dr. Yelena Kann, senior polymer scientist at Metabolix, will report on "New Biobased PHA Rubber Copolymers for PVC Modification" at the Society of Plastics Engineers' Vinyltec 2012 conference tomorrow in Chicago.

"PHA could significantly simplify PVC compound formulation by replacing secondary plasticizers, replacing or reducing amount of primary plasticizers, replacing impact modifiers, eliminating the need for the shear promoting processing aid, eliminating UV stabilizers," Dr.Kann tells Plastics Today. 

Potential cost savings

PHAs also potentially offers cost savings due to their multifunctional performance. Loadings would range from 5 phr to 30 phr of PHA in PVC.

PHAs also improved impact modification in PVC. According to Dr. Kann, PHA rubber copolymers outperformed the best available MBS core/shell impact modifiers and did not compromise PVC transparency or UV stability. The metal-adhering properties of PHA copolymers also promoted homogeneous shear melting of PVC particles and prevented overheating and degradation.

"The significant performance benefits PVC gained from blending with PHA copolymers underscores the versatility and value of Metabolix's PHA technology," said Oliver Peoples, chief scientific officer and vice president of research at Metabolix. "These developments will allow us to broaden the addressable market opportunity for our materials, beyond our traditional focus on those markets requiring biodegradation."

Metabolix worked with AlphaGary (Leominster, MA), custom compounder of PVC and TPE/TPO materials, to study PHA polymeric modifiers in PVC.

"We are pleased with what we have seen in these new polymeric PVC modifiers and are beginning to test them in current high-value applications. They combine effective impact modification with good transparency and are made from renewable feedstocks," said Mark Jozokos, global R&D manager at AlphaGary.

Metabolix plans to manufacture the new PHA products in a10,000 tonnes per year facility in Leon, Spain. Samples of the polymeric modifiers will be available to ship to customers in early 2013. Last July, Metabolix announced a manufacturing relationship with Antibióticos S.A., a producer of active pharmaceutical ingredients using fermentation processes.

Metabolix needed to find a new production partner for its PHAs after Archer Daniels Midland Company (ADM) terminated a JV called Telles in February due to concerns about the financial prospects for the project.

Metabolix  was formed in 1992 to commercialize genetically engineered production organisms developed in the MIT lab of Dr. Anthony Sinskey by Oliver Peoples. The company also bought Monsanto patents for PHA bioplastics, including Biopol.