The Micropoint hot runner nozzle, designed to service small part hot runner molding applications, has a special alloy tip design to process engineering and glass-filled resins without deteriorating the tip. It allows easy serviceability and can be easily replaced if needed along with the heater and thermocouple.
The small size of the Micropoint makes it suitable for small molds and part shot sizes, while also allowing for low residence time of the resin, accurate volume shot size, and consistent straight heat profile. The manufacturer's Flat Gate System allows the customization of each design for a particular customer's needs. Prices were not made available.