MicroGREEN launches InCycle sheet product at Pack ExpoMicroGREEN launches InCycle sheet product at Pack Expo
Tapping into another potentially huge market, MicroGREEN Polymers Inc. (Seattle, WA) is now promoting its patented technology, which maximizes the use of recycled plastics through the addition of tiny air pockets, into the packaging sector with its new sheet offering dubbed InCycle.
November 9, 2010

(Seattle, WA) is now promoting its patented technology, which maximizes the use of recycled plastics through the addition of tiny air pockets, into the packaging sector with its new sheet offering dubbed InCycle. Launched at Pack Expo in Chicago, InCycle sheet, based on recycled polyethylene terephthalate (PET) was on display as thermoformed and convolute cups, convolute overwraps, printed flat sheet, blister pack cards, thermoformed trays, and folded boxes, clamshells, and other food-service containers.