Researchers Devise Rapid 3D Printing Method for Human Organs

Use of hydrogels in novel stereolithography process eyed for fabricating viable tissues for transplants and other biomedical applications.

3 Min Read
Feature AdobeStock_312072145.jpeg
Adobe Stock

The Holy Grail of 3D bioprinting is to one day be able to fabricate full-sized human organs and tissues to replace the real thing in cases of transplant surgeries and other biomedical applications.

Researchers at the University at Buffalo have made a significant step not only to achieve this endeavor but to do it quickly. A team of researchers there has developed 3D-printing technology that has demonstrated rapid printing of life-sized organs and limbs such as a human hand in less than 20 minutes.

The team—co-led by Ruogang Zhao, associate professor of biomedical engineering, and Chi Zhou, associate professor of industrial and systems engineering—created a 3D-printing method based on stereolithography that uses hydrogels to produce organs quickly. Hydrogels are materials comprised mainly of water that are already used to produce contact lenses and diapers as well as in other applications.

“Our method allows for the rapid printing of centimeter-sized hydrogel models” that “significantly reduces part deformation and cellular injuries caused by the prolonged exposure to the environmental stresses you commonly see in conventional 3D printing methods,” Zhou said in a press statement.

How It Works

That method is called fast hydrogel stereolithography printing (FLOAT), which allows for the creation of a centimeter‐sized, multiscale solid hydrogel model within minutes. The idea is that this technology can be used to produce life-like tissue samples and organs as needed, which would provide a solution to the shortage of organs available for those needing transplants, researchers said.

Related:New Platform Combines 3D Printing and Injection Molding to Produce Flexible Parts

While the printing of “large size cell‐laden hydrogel models hold great promise for tissue repair and organ transplantation, their fabrication using 3D bioprinting is limited by the slow printing speed that can affect the part quality and the biological activity of the encapsulated cells,” researchers wrote in an abstract for a paper on the work published in the journal Advanced Healthcare Materials.

Researchers developed the method by precisely controlling the photopolymerization condition of the process to create a low-suction, force‐driven, high‐velocity flow of a hydrogel prepolymer. “This supports the continuous replenishment of the prepolymer solution below the curing part and the nonstop part growth,” they wrote.

By controlling the printing process in this way, FLOAT can produce parts without the usual stress and deformation that other 3D-printing methods can produce, particularly in rapid-fabrication scenarios, Zhao said.

Related:3D Printing and Modeling Crucial to Face and Hands Transplant

“The technology we’ve developed is 10-50 times faster than the industry standard, and it works with large sample sizes that have been very difficult to achieve previously,” he said in a press statement.

Moreover, the process can be used to print living cells embedded with vascular or blood-vessel networks, a nascent technology that are expected to be an integral part of the production of 3D-printed human tissue and organs. These networks are a part of the connective infrastructure that provides viability for these fabricated organs to function like the real thing, researchers said.

3dprintliver (002).jpg

The team published a video that demonstrates how their FLOAT rapid bioprinting method works. They also have filed a provisional patent of the technology, as well as formed a startup company, Float3D, to commercialize it.

Elizabeth Montalbano is a freelance writer who has written about technology and culture for more than 20 years. She has lived and worked as a professional journalist in Phoenix, San Francisco, and New York City. In her free time, she enjoys surfing, traveling, music, yoga, and cooking. She currently resides in a village on the southwest coast of Portugal.

About the Author(s)

Elizabeth Montalbano

Elizabeth Montalbano has been a professional journalist covering the telecommunications, technology and business sectors since 1998. Prior to her work at Design News, she has previously written news, features and opinion articles for Phone+, CRN (now ChannelWeb), the IDG News Service, Informationweek and CNNMoney, among other publications. Born and raised in Philadelphia, she also has lived and worked in Phoenix, Arizona; San Francisco and New York City. She currently resides in Lagos, Portugal. Montalbano has a bachelor's degree in English/Communications from De Sales University and a master's degree from Arizona State University in creative writing.

Sign up for the PlasticsToday NewsFeed newsletter.

You May Also Like